반응식
[CH2:1]=[C:2]=[CH2:3].[C:4]1([C:10]#[CH:11])[CH:9]=[CH:8][CH:7]=[CH:6][CH:5]=1.C=C=C.C#CC>CO>[CH2:1]=[C:2]=[CH2:3].[C:4]1([C:10]#[CH:11])[CH:9]=[CH:8][CH:7]=[CH:6][CH:5]=1참가 물질
5
반응 조건
- 온도
- 60 °C
실험 절차
In this example the starting monomers allene and phenylacetylene (HC≡C--O) are introduced into the catalyst mixture of Example 1 in a feed ratio of 62 to 38 (mole ratio). The polymerization conditions and catalyst are the same as in Example 1. After stirring at 60° C. for ten hours, a copolymer with a molecular weight of about 25,000 daltons (measured by GPC) is produced and can be isolated by precipitation to methanol. Given a starting amount of 0.5 g allene and 1.18 g phenylacetylene, the yield of copolymer will be 1.5 g, and have the formula: ##STR13##
후처리
- customThe polymerization conditions and catalyst
- customa copolymer with a molecular weight of about 25,000 daltons (measured by GPC) is produced
출처 및 근거
- ORD 기록
- ord-6c267fdb1d9f4bf690b4a64c6c6aacaf
- 출처 데이터셋
- uspto-grants-1998_05
- 특허 번호
- US05747618
연결된 노트
불러오는 중…