Maleic Anhydride → Octadecene maleate

HRID 1388759

반응식

HRID 1388759 반응식
[OH-].[Na+].[CH2:3]=[CH:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH2:16][CH2:17][CH2:18][CH2:19][CH3:20].[C:21]1(=[O:27])[O:26][C:24](=[O:25])[CH:23]=[CH:22]1.C=CCCCCCCCCCCCCCCCC.C1(=O)OC(=[O:50])C=C1>[Cl-].C([N+](CCCCCCCCCCCCCCCCCC)(C)C)CCCCCCCCCCCCCCCCC.O>[CH2:3]=[CH:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH2:16][CH2:17][CH2:18][CH2:19][CH3:20].[C:21]([O-:26])(=[O:27])/[CH:22]=[CH:23]\[C:24]([O-:50])=[O:25]

참가 물질

7

반응 조건

온도
85 °C

실험 절차

The ion pair of the distearyl dimethyl ammoniun cation and the octadecene-maleate copolymer anion was prepared as follows. 4 g (0.05 mole) of 50% NaOH was added to 100 ml of water and 29.3 g (0.05 moles) of distearyl dimethyl ammonium chloride was dispersed in the mixture. It was heated to 85° C. and 8.8 g (0.05 moles of carboxylate) of 1:1 copolymer of octadecene and maleic anhydride was added as a powder. The mixture was stirred at 85° to 90° C. for 10 hours, during which the octadecene-maleic anhydride copolymer particles disappeared. The water phase gradually cleared and gelled particles of the ion pair formed. The product was separated by decanting the water. The product weighed 57.5 g and contained 36.1% water. The remaining water was removed by spreading the gelled product in a thin layer and passing air at room temperature across it. It was ground in a Waring Blender to a fine non-tacky powder.

후처리

  1. additionwas dispersed in the mixture
  2. customformed
  3. customThe product was separated
  4. customby decanting the water
  5. customThe remaining water was removed
  6. customat room temperature

출처 및 근거

ORD 기록
ord-c11fec557f5e4bb4b99c7fb5d3b98289
출처 데이터셋
uspto-grants-1984_02
특허 번호
US04433113