반응식
Br[C:2]1[CH:8]=[CH:7][C:5]([NH2:6])=[CH:4][CH:3]=1.[C:9]1(B(O)O)[C:18]2[C:13](=[CH:14][CH:15]=[CH:16][CH:17]=2)[CH:12]=[CH:11][CH:10]=1.C1(C)C=CC=CC=1P(C1C=CC=CC=1C)C1C=CC=CC=1C.C(=O)([O-])[O-].[K+].[K+]>C([O-])(=O)C.[Pd+2].C([O-])(=O)C.O.C1(C)C=CC=CC=1.C(O)C>[C:17]1([C:2]2[CH:8]=[CH:7][C:5]([NH2:6])=[CH:4][CH:3]=2)[C:18]2[C:13](=[CH:12][CH:11]=[CH:10][CH:9]=2)[CH:14]=[CH:15][CH:16]=1참가 물질
반응 조건
- 온도
- 60 °C
실험 절차
First, 5.0 g (29 mmol) of 4-bromoaniline, 5.0 g (29 mmol) of 1-naphthylboronic acid, and 0.45 g (1.5 mmol) of tri(ortho-tolyl)phosphine were put into a 500-mL three-neck flask, and the air in the flask was replaced with nitrogen. Then, 100 mL of toluene, 50 mL of ethanol, and 31 mL of a potassium carbonate aqueous solution (2 mol/L) were added to this mixture. The mixture in the flask was stirred and degassed while reducing pressure in the flask. Then, after the mixture was heated at 60° C., 66.2 mg (0.29 mmol) of palladium(II) acetate was added to the mixture. The mixture was refluxed at 80° C. for 2.3 hours. After the reflux, toluene and water were added to the mixture, an organic layer and an aqueous layer were separated, and the aqueous layer was extracted twice with toluene. The extract and the organic layer were combined, washed with a saturated saline solution, and dried with magnesium sulfate. The mixture was subjected to gravity filtration to remove magnesium sulfate. Then, the filtrate was concentrated to give an oily substance, which was subjected to suction filtration through Florisil (produced by Wako Pure Chemical Industries, Ltd., Catalog No. 540-00135), Celite (produced by Wako Pure Chemical Industries, Ltd., Catalog No. 531-16855), and alumina to obtain a filtrate. The resulting filtrate was concentrated to give 2.5 g of an oily substance, which was an object, in a yield of 40%.
후처리
- customdegassed
- temperatureThe mixture was refluxed at 80° C. for 2.3 hours
- customan organic layer and an aqueous layer were separated
- extractionthe aqueous layer was extracted twice with toluene
- extractionThe extract
- washwashed with a saturated saline solution
- dry with materialdried with magnesium sulfate
- filtrationThe mixture was subjected to gravity filtration
- customto remove magnesium sulfate
- concentrationThen, the filtrate was concentrated
- customto give an oily substance, which
- filtrationwas subjected to suction filtration through Florisil (produced by Wako Pure Chemical Industries, Ltd., Catalog No. 540-00135), Celite (produced by Wako Pure Chemical Industries, Ltd., Catalog No. 531-16855), and alumina
- customto obtain a filtrate
- concentrationThe resulting filtrate was concentrated
- customto give 2.5 g of an oily substance, which