홈MCP워크벤치Skills
홈워크벤치알림마이페이지
llms.txt · MCP 가이드개인정보처리방침 · 이용약관 · 지원v1.8.3
  1. 홈
  2. /반응

Ethylenediaminetetraacetic Acid → Styrene

HRID 1512721
인쇄

반응식

HRID 1512721 반응식
[O-]O.[CH:3]1(C)[CH2:8][CH2:7][CH:6]([CH:9](C)[CH3:10])[CH2:5][CH2:4]1.S([O-])[O-].C=O.[Na+].[Na+].C(N(CC(O)=O)CC(O)=O)CN(CC(O)=O)CC(O)=O>>[CH2:8]=[CH:3][CH:4]=[CH2:5].[CH2:10]=[CH:9][C:6]1[CH:7]=[CH:8][CH:3]=[CH:4][CH:5]=1
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

5

반응물 3

HCID 6049Ethylenediaminetetraacetic AcidHCID 21225536CID 21225536HCID 86641008Paramenthane hydroperoxide2회

생성물 2

HCID 7501StyreneHCID 78451,3-Butadiene

실험 절차

0.015 part of paramenthane hydroperoxide and subsequently 0.04 part of sodium formaldehyde sulfoxylate were introduced into the system to initiate polymerization. Four hours later from the initiation of polymerization, 0.01 part of paramenthane hydroperoxide, 0.0015 part of ethylenediamine tetraacetic acid and 0.001 part of ferrous sulfate were introduced. Ten hours later from the initiation of polymerization, residual monomers were removed by deaeration under reduced pressure, and the polymerization was completed. Thus, rubber latex containing rubbery polymer particles obtained by copolymerizing 75% by weight of butadiene and 25% by weight of styrene was prepared.

후처리

  1. custompolymerization
  2. additionwere introduced
  3. customTen hours later from the initiation of polymerization, residual monomers
  4. customwere removed by deaeration under reduced pressure
  5. additionThus, rubber latex containing rubbery polymer particles