Ammonia → Acrylamide-acrylic acid resin

HRID 1589241

반응식

HRID 1589241 반응식
[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].N.[C:7]([NH2:11])(=[O:10])[CH:8]=[CH2:9]>O>[C:1]([OH:5])(=[O:4])[CH:2]=[CH2:3].[C:7]([NH2:11])(=[O:10])[CH:8]=[CH2:9]

참가 물질

5

실험 절차

To a stainless steel beaker was charged 214 g. of glacial acrylic acid (Rohm and Haas Production Grade). While stirring with a magnetic stirrer, 29% aqueous ammonia (technical) was added and the temperature was maintained at ≤35° C. until the pH became 7.5 (about 1.5 hours). Distilled water was added to bring the total weight to 428 g. The solution was transferred to a 1 liter glass beaker and while stirring 1.07 g. of methone was added (0.5% based on the acrylic acid). It dissolved in about 10 minutes. Then 23 g. of 50% acrylamide was added and the procedure of Examples 29-38 was followed to emulsion polymerize the monomers.

후처리

  1. temperaturethe temperature was maintained at ≤35° C. until the pH
  2. custom7.5 (about 1.5 hours)
  3. stirringwhile stirring 1.07 g
  4. additionof methone was added (0.5%
  5. dissolutionIt dissolved in about 10 minutes
  6. custompolymerize the monomers

출처 및 근거

ORD 기록
ord-9f5b74bbd6364ac683a742da4d0ffb71