반응식
[C:1]1(=[O:7])[O:6][C:4](=[O:5])[CH:3]=[CH:2]1.[C:8]([O:11][CH:12]=[CH2:13])(=[O:10])[CH3:9].C(OOC(C)(C)C)(C)(C)C>C1(C)C(C)=CC=CC=1>[C:4]1(=[O:5])[O:6][C:1](=[O:7])[CH:2]=[CH:3]1.[C:8]([O:11][CH:12]=[CH2:13])(=[O:10])[CH3:9]참가 물질
5
반응 조건
- 온도
- 70 °C
실험 절차
73.5 parts by weight of maleic anhydride and 21.4 parts by weight of vinyl acetate were dissolved in 240 parts by volume of xylene and heated to 70° C. 4.5 parts by weight of ditertiary butyl peroxide in 20 parts by volume of xylene were added and the reaction mixture was heated to 130° C. and maintained at this temperature for 3 hours. A brown resin precipitated, which on cooling solidified, and was easily separated from the bulk of the xylene by decantation. Yield = 87% (on weight of monomers). The number average molecular weight of the polymer by vapour phase osmometry was found to be 675.
후처리
- temperaturethe reaction mixture was heated to 130° C.
- temperaturemaintained at this temperature for 3 hours
- customA brown resin precipitated
- temperaturewhich on cooling solidified
- customwas easily separated from the bulk of the xylene by decantation