[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:14]([NH2:18])(=[O:17])[CH:15]=[CH2:16].[C:19]([O:22][CH:23]=[CH2:24])(=[O:21])[CH3:20].N(C(C)(CC(C)C)C#N)=NC(C)(CC(C)C)C#N.CC(N=NC(C#N)(C)C)(C#N)C>C(OCC)(=O)C.CO.C(OCC)(=O)C.CO>[C:14]([NH2:18])(=[O:17])[CH:15]=[CH2:16].[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:19]([O:22][CH:23]=[CH2:24])(=[O:21])[CH3:20]참가 물질
반응물 5
생성물 1
시약·촉매·용매 3
실험 절차
A master batch was prepared by combining 621.0 g of isooctyl acrylate, 41.4 g of acrylamide, 165.6 g of vinyl acetate, 1.656 g of 2,2′-azobis(2,4-dimethylpentanenitrile) (available from the DuPont Company as Vazo™ 52), 884.52 g of ethyl acetate and 87.48 g of methanol. A 400 g portion of the resulting solution was placed in an amber quart bottle. The bottle was purged for two minutes with nitrogen at a flow rate of one liter per minute. The bottle was sealed and placed in a rotating water bath at 45° C. for twenty-four hours to effect essentially complete polymerization. The copolymer was diluted with 250 g of ethyl acetate/methanol (90/10) to 26.05% solids and had a measured inherent viscosity of 1.27 dl/g in ethyl acetate at a concentration of 0.15 g/dl. Its Brookfield viscosity was 5580 centipoise.
후처리
- customA master batch was prepared
- customThe bottle was purged for two minutes with nitrogen at a flow rate of one liter per minute
- customThe bottle was sealed
- waitplaced in a rotating water bath at 45° C. for twenty-four hours
- custompolymerization