Ethylene carbonate → Ethylene carbonate

HRID 247715

반응식

HRID 247715 반응식
[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1>O.O.O.[O-][Sn]([O-])=O.[Na+].[Na+]>[C:1]1(=[O:6])[O:5][CH2:4][CH2:3][O:2]1.[C:1](=[O:5])=[O:2]

참가 물질

4

반응 조건

온도
175 °C

실험 절차

A 10:1 mole ratio of ethylene carbonate to polyester polyol (poly(caprolactone) diol, MW=530) is heated with stirring under a nitrogen atmosphere for 4 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 97.9 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 19.2 percent carbon dioxide. The catalyst is removed as in Example 1.

출처 및 근거

ORD 기록
ord-83e27cce764c40d789da328866ec9e7a
출처 데이터셋
uspto-grants-1987_11
특허 번호
US04709069

연결된 노트