반응식
[Cl-].[Ca+2:2].[Cl-].[O-:4][P:5]([O:8][P:9]([O-:12])([O-:11])=[O:10])(=[O:7])[O-:6].[Na+].[Na+].[Na+].[Na+]>>[O-:6][P:5]([O:8][P:9]([O-:12])([O-:11])=[O:10])(=[O:4])[O-:7].[Ca+2:2].[Ca+2:2]참가 물질
3
실험 절차
However, when 150 mM calcium chloride solution and 75 mM tetrasodium pyrophosphate solution, both adjusted to pH 7, were used to form the initial mixture, very small fibrous calcium pyrophosphate particles with a diameter of about 1 to 3 microns were formed. Similar results were obtained when 75 mM calcium chloride solution and 37.5 mM tetrasodium pyrophosphate solution were used to form the initial mixture.
출처 및 근거
- ORD 기록
- ord-3b721d408c9a47fe82ab66a394770963
- 출처 데이터셋
- uspto-grants-2014_11
- 특허 번호
- US08889745B2
연결된 노트