Ethyl Acetate → Isooctyl Acrylate 2-Hydroxyethyl Acrylate

HRID 350591

반응식

HRID 350591 반응식
[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:14]([O:18][CH2:19][CH2:20][OH:21])(=[O:17])[CH:15]=[CH2:16].N(C(C)(CC)C#N)=NC(C)(CC)C#N.C(OCC)(=O)C>C(O)(C)C>[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:14]([O:18][CH2:19][CH2:20][OH:21])(=[O:17])[CH:15]=[CH2:16]

참가 물질

6

실험 절차

A master batch was prepared by combining isooctyl acrylate (714.00 g), 2-hydroxyethyl acrylate (523.00 g), polymethylmethacrylate macromonomer (52.00 g) of ELVACITE™ 1010 available from ICI Acrylics), 2,2′-azobis(2-methylbutyronitrile) (2.60 g), ethyl acetate (1245.50 g) and isopropanol (45.50 g). The resulting solution was divided in equal portions and placed into six 1 quart (0.95 L) amber glass bottles. The bottles were purged for 2 minutes with nitrogen at a flow rate of 1 L per minute. The bottles were sealed and placed in a rotating water bath at 57° C. for 24 hours. At 24 hours the bottles were removed from the rotating water bath, unsealed, diluted with 76 g methanol per bottle, mixed until homogenous, and recombined into a 1 gallon (3.8 L) glass jar. The percent solids of the resultant copolymer was 40.5%. The inherent viscosity, I.V., (of a 0.15 g/dL solution of polymer in ethyl acetate measured at 27° C.) was 0.77 dL/g.

후처리

  1. customA master batch was prepared
  2. customThe bottles were purged for 2 minutes with nitrogen at a flow rate of 1 L per minute
  3. customThe bottles were sealed
  4. customAt 24 hours the bottles were removed from the rotating water bath
  5. additionunsealed, diluted with 76 g methanol per bottle
  6. additionmixed until homogenous, and
  7. custommeasured at 27° C.

출처 및 근거

ORD 기록
ord-e679dc1663a944ff874dc5589c13b392
출처 데이터셋
uspto-grants-2007_02
특허 번호
US07182955B2

연결된 노트

불러오는 중…