반응식
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH2:9]=[CH:10][CH:11]=[CH2:12].CN(CCN(C)C)C.[Li]CCCC>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH2:9]=[CH:10][CH:11]=[CH2:12]참가 물질
5
실험 절차
In this example, a 1/11/88 PES/styrene/1,3-butadiene terpolymer was prepared using the procedure described in Example 34 except that the ratio of PES to styrene and to 1,3-butadiene was changed to 1:11:80 and the molar ratio of TMEDA to n-BuLi was also changed to 1:1. GC analysis of residual monomer with respect to polymerization time indicated that PES was randomly distributed along the polymer chain. The resulting terpolymer had a Tg at −42° C. and was determined to a have a ML-4 of 47.
후처리
- customGC analysis of residual monomer with respect to polymerization time
- customat −42° C.
출처 및 근거
- ORD 기록
- ord-53e0851c347d4509bc52251a0e84c4f5
- 출처 데이터셋
- uspto-grants-2004_06
- 특허 번호
- US06753447B2
연결된 노트
불러오는 중…