[CH2:1]1[CH2:6]CC[CH2:3][CH2:2]1.[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1.C([Li])CCC.C=CC=C>O1CCCC1>[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1.[CH2:6]=[CH:1][CH:2]=[CH2:3].[CH2:7]=[CH:8][C:9]1[CH:14]=[CH:13][CH:12]=[CH:11][CH:10]=1참가 물질
실험 절차
In a 2 gallon autoclave reactor, 4,500 g of cyclohexane was placed. 9 g of tetrahydrofuran, 112.5 g of styrene monomer and 1.6 g of n-butyllithium were charged into the reactor and then the reaction mixture was subjected to polymerization for 1 hour. Thereafter, 525 g of 1,3-butadiene monomer were injected into the reactor to polymerize for one hour. Finally, 112.5 g of styrene monomer was added and then polymerized for one hour to obtain styrene-butadiene-styrene living block copolymer with a number average molecular weight of about 60,000 which had a styrene content of 30.54% (block styrene content of 30.3%) and 1,2-vinyl bond content of 39.80% (27.8% when reduced into whole polymer). Living lithium in the polymer was present in an amount of 1.67 mmol per 100 g of polymer.
후처리
- customthe reaction mixture was subjected to polymerization for 1 hour
- customto polymerize for one hour
- custompolymerized for one hour
출처 및 근거
- ORD 기록
- ord-b0b4f16fa166401598cc7b31c770170f
- 출처 데이터셋
- uspto-grants-2000_02
- 특허 번호
- US06020439
연결된 노트
불러오는 중…