[C:1]([O:6][CH2:7][CH:8]=[CH:9][C:10]1[CH:15]=[CH:14][CH:13]=[CH:12][CH:11]=1)(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:16]([O:21][C:22]1[C:31]2[C:26](=[CH:27][CH:28]=[CH:29][CH:30]=2)[CH:25]=[CH:24][CH:23]=1)(=[O:20])[C:17]([CH3:19])=[CH2:18].C(OCC1C=CC(COC(=O)C=C)=CC=1)(=O)C=C.COC(C1C=CC=CC=1)C(=O)C1C=CC=CC=1.N(C1CCCCC1)=O>ClC1C2C(=CC=CC=2)C=CC=1.C1C=CC=CC=1.C1(C)C(C)=CC=CC=1>[C:1]([O:6][CH2:7][CH:8]=[CH:9][C:10]1[CH:11]=[CH:12][CH:13]=[CH:14][CH:15]=1)(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:16]([O:21][C:22]1[C:31]2[C:26](=[CH:27][CH:28]=[CH:29][CH:30]=2)[CH:25]=[CH:24][CH:23]=1)(=[O:20])[C:17]([CH3:19])=[CH2:18]참가 물질
9
반응물 5
생성물 1
시약·촉매·용매 3
실험 절차
A mixture of 2.00 g poly(cinnamyl methacrylate/-1-naphthyl methacrylate), 1.50 g 1-naphthyl methacrylate, 0.25 g p-xylylene diacrylate, 0.40 g benzoin methyl ether, 0.05 g 20% nitrosocyclohexane dimer in 1-chloronaphthalene, and 3.00 g xylene was prepared. Poly(cinnamyl methacrylate/1-naphthyl methacrylate) was prepared by thermally copolymerizing equal parts of cinnamyl methacrylate and 1-naphthyl methacrylate in a benzene solution using an azonitrile initiator. The polymer was precipitated from solution and washed prior to use.
후처리
- customThe polymer was precipitated from solution
- washwashed
출처 및 근거
- ORD 기록
- ord-9a576419313945b99d3a9a36026ccab0
- 출처 데이터셋
- uspto-grants-1977_02
- 특허 번호
- US04008083
연결된 노트
불러오는 중…