홈MCP워크벤치Skills
홈워크벤치알림마이페이지
llms.txt · MCP 가이드개인정보처리방침 · 이용약관 · 지원v1.8.3
  1. 홈
  2. /반응

Methacrylic Acid → 2-Propenoic acid, butyl ester, polymer with 2-ethylhexyl 2-propenoate

HRID 462806
인쇄

반응식

HRID 462806 반응식
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9]([O:14][CH2:15][CH2:16][CH2:17][CH3:18])(=[O:13])[C:10](C)=[CH2:11].C(OCC)(=O)C(C)=C.C(O)(=O)C(C)=C>C1(C)C=CC=CC=1>[CH3:5][CH2:6][CH2:7][CH2:8][CH:3]([CH2:4][O:14][C:9]([CH:10]=[CH2:11])=[O:13])[CH2:2][CH3:1].[CH3:18][CH2:17][CH2:16][CH2:15][O:14][C:9]([CH:10]=[CH2:11])=[O:13]
참가 물질반응 조건실험 절차후처리출처 및 근거반응 노트

참가 물질

6

반응물 4

HCID 4093Methacrylic AcidHCID 7343Ethyl MethacrylateHCID 7354Butyl MethacrylateHCID 7501Styrene

생성물 1

HCID 1685972-Propenoic acid, butyl ester, polymer with 2-ethylhexyl 2-propenoate

시약·촉매·용매 1

HCID 1140Toluene용매3회

반응 조건

온도
110 °C

실험 절차

An acrylic copolymer resin was prepared by feeding 150 parts of toluene into a 500-ml 4-necked flask equipped with a cooling tube, stirrer, and thermometer, heating it to 110° C., adding styrene 20 parts, n-butyl methacrylate 60 parts, ethyl methacrylate 120 parts, methacrylic acid 14 parts, azoisobutyronitrile 5 parts and toluene 70 parts spending 2 hours under an inert gas atmosphere, and heating for further 6 hours. The resulting toluene solution of copolymer was found to have 50.5% of nonvolatile matter and a polymer acid value of 18.

후처리

  1. customequipped with a cooling tube, stirrer
  2. temperatureheating for further 6 hours

출처 및 근거

ORD 기록
ord-857d26fa16d844279ad74f97e21ea440
출처 데이터셋
uspto-grants-1985_05
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US04517271

반응 노트

이 페이지에서참가 물질반응 조건실험 절차후처리출처 및 근거반응 노트