반응식
[C:1]([P:4](=[O:7])([OH:6])[OH:5])([CH3:3])=[CH2:2].[OH:8][CH2:9][CH2:10][O:11][C:12](=[O:16])[C:13]([CH3:15])=[CH2:14].S(OOS([O-])(=O)=O)([O-])(=O)=O.[NH4+].[NH4+]>O>[C:1]([P:4](=[O:5])([OH:7])[OH:6])([CH3:3])=[CH2:2].[OH:8][CH2:9][CH2:10][O:11][C:12](=[O:16])[C:13]([CH3:15])=[CH2:14]참가 물질
5
실험 절차
Aqueous isopropenyl phosphonic acid (71 g, 54%, 0.3 mole) and hydroxyethylmethacrylate (13 g, 0.1 mole) were mixed with 121.6 g water in a resin kettle. Ammonium persulfate (6 g) was added. After 11/2 hours of reflux, an additional 6 g of initiator was added followed by another 11/2 hours of reflux. The final product was a yellow solution with a pH of 0.68. The 31PMR showed polymeric absorptions centered at δ=-29.5 and -24.3 ppm.
후처리
- temperatureAfter 11/2 hours of reflux
- custom2 hours
- temperatureof reflux
출처 및 근거
- ORD 기록
- ord-83e7242a4dca444995cd572292ecdc81
- 출처 데이터셋
- uspto-grants-1984_05
- 특허 번호
- US04446028
연결된 노트