[O-2].[O-2].[O-2].[O-2].[O-2].[V+5:6].[V+5].[C:8]([OH:13])(=[O:12])[C:9]([OH:11])=[O:10]>O>[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[V+5:6].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[C:8]([O-:13])(=[O:12])[C:9]([O-:11])=[O:10].[V+5:6]참가 물질
4
반응 조건
- 온도
- 1300 °C
실험 절차
Granulated alumina (8 - 16 mesh) is heated at 1300° C. for 4 hours. Ferric oxalate and vanadium pentoxide are suspended in 5 parts of water, heated to 80° C., and oxalic acid is added slowly to obtain a blue-colored vanadium oxalate solution. Sodium carbonate is added and the alumina is also placed in the solution. The mixture is dried over a water bath with agitation. While air is pumped in, it is indurated in a furnace at 400° C. for 16 hours to obtain the catalyst ready for use after cooling.
후처리
- temperatureheated to 80° C.
출처 및 근거
- ORD 기록
- ord-1c8d8fde67494fee931bb436573a4fa7
- 출처 데이터셋
- uspto-grants-1977_03
- 특허 번호
- US04013705
연결된 노트
불러오는 중…