실험 절차
A method for producing submicron-sized particles of zinc pyrithione, comprising reacting a pyrithione or a water-soluble salt of pyrithione and a water-soluble zinc salt selected from the group consisting of zinc sulfate, zinc chloride, zinc acetate, and combinations thereof, in a turbulent flow reactor generating pulverizing forces, said turbulent flow reactor maintained at a pressure of from about 18,000 psi to about 23,000 psi and a temperature of from about 0° C. to about 23° C., said reaction producing submicron-sized particles of zinc pyrithione.
후처리
- customin a turbulent flow reactor generating pulverizing
- temperaturemaintained at a pressure of from about 18,000 psi to about 23,000 psi
- customof from about 0° C. to about 23° C.
- customreaction
출처 및 근거
- ORD 기록
- ord-78d2d706ef0b4b23ad56fef5cffc7d60
- 출처 데이터셋
- uspto-grants-2000_01
- 특허 번호
- US06017936
연결된 노트
불러오는 중…