HRID1007063

反应详情

EQUATION

反应方程式

HRID 1007063 的结构方程式

PROCEDURE

实验过程

3-Hydroxyadamantyl methacrylate and 4-acetoxystyrene were charged at a charge ratio of 2:8 to synthesize a base resin. The resin obtained was treated with an alkali solution to cause soluvolysis of the acetyl group, thereby obtaining a 3-hydroxyadamantyl methacrylate-vinylphenol copolymer (molecular weight: 4,500). To polyvinylphenol produced by Maruzen Sekiyu, 15 wt % of the copolymer obtained was added and the mixture was dissolved in PGMEA (propylene glycol methyl ether acetate). To this solution, 5 wt % of triphenylsulfoium trifluoromethanesulfonate was added and thoroughly dissolved. The thus-obtained resist solution was filtered through a 0.2 μm teflon membrane filter, spin-coated on a silicon substrate subjected to an HMDS treatment, and pre-baked at 110° C. for 60 seconds to form a 0.5 μm-thick resist film. This resist film was exposed by a KrF excimer laser stepper (NA=0.45), baked at 120° C. for 60 seconds, developed with a 2.38% tetramethylammonium hydroxide (TMAH) developer, and rinsed with deionized water. With an exposure amount of 12.0 mJ/cm2, a resolution of 0.25 μmL/S was obtained. In this resist pattern, swelling was not generated.

WORKUP

后处理

  1. customto synthesize a base resin
  2. customThe resin obtained
  3. additionwas treated with an alkali solution