Propylene Carbonate → 2-Hydroxyethyl Methacrylate

HRID 1067157Notes

Reaction equation

HRID 1067157 reaction equation
[C:1]1(C2C=[N+](CCC)C=CC=2C2C=C[NH+]=CC=2)[CH:6]=CC=C[CH:2]=1.[C:22]1(=[O:28])[O:27][CH:25](C)[CH2:24][O:23]1>CC1C=CC(O)=C(N2N=C3C(C=CC=C3)=N2)C=1.CN1C2C(=CC=CC=2)N(C)C2C=CC=CC1=2>[CH3:6][C:1]([C:22]([O:23][CH2:24][CH2:25][OH:27])=[O:28])=[CH2:2]

Participants

5

Procedure

The pre-polymer solution of Example 13 A was diluted to 7% by weight polymer with propylene carbonate. The pre-polymer solution was made 30 millimolar in Tinuvin p, 17 millimolar in 1,1′-d-(3-phenyl(n-propyl)-4,4′ bipyridinium and 14 millimolar in 5,10-dihydro-5,10-dimethlphenazine simply by dissolving appropriate amounts of these materials in the pre-polymer solution. This solution was degassed by vacuum and flushed with nitrogen. Sufficient tolylene 2,4-diisocyanate (available from Aldrich Chemical Company, Inc. Milwaukee, Wis.) crosslinker was added to crosslink approximately 50 percent of the theoretical hydroxyl position. This solution was thoroughly mixed to ensure that the crosslinker was evenly distributed throughout the fluid.

Workup

  1. customThis solution was degassed by vacuum
  2. customflushed with nitrogen
  3. additionSufficient tolylene 2,4-diisocyanate (available from Aldrich Chemical Company, Inc. Milwaukee, Wis.) crosslinker was added
  4. additionThis solution was thoroughly mixed

Sources & evidence

ORD record
ord-faf9d11cf5d74137998d8abfcb062357
Source dataset
uspto-grants-2001_06
Patent number
US06248263B1

Reaction notes

Loading…