Aluminum Stearate → Ethylene brassylate

https://huagongshe.com/reaction/1074627

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAluminum StearateHCID 12496—
ReactantLithium StearateHCID 517357—
ProductEthylene brassylateHCID 6101488.9%

Reaction Conditions

Temperature314 °C

Reaction Steps

A mixed metal catalyst comprised of aluminum stearate and lithium stearate (molar ratio 1:1) was used for the depolymerization. For the reaction aluminum stearate (1.09 g) and lithium stearate (0.36 g) were blended in 70 g poly(ethylene brassylate) at 200° C. The temperature was then raised to 314° C. while maintaining a vacuum of 0.05-0.1 mm Hg. Ethylene brassylate was obtained (40 mls during the first hour) in an 88.9% yield. Of the ethylene brassylate recovered, 90% of the product was obtained after 2 hours.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04393223
Source datasetuspto-grants-1983_07
ORD IDord-87f4e281078c4305b7525009f18c66b4
Source noteuspto-grants-1983_07