Styrene → 2-Methylbuta-1,3-diene;styrene

HRID 1075685Notes

Reaction equation

HRID 1075685 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[Li]CCCC>>[CH2:1]=[CH:2][C:3](=[CH2:4])[CH3:8].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

3

Procedure

The procedure described in Example 9 was utilized in this example except that a premix containing 25:75 mixture of styrene and 1,3-isoprene in hexanes was used in place of isoprene and the modifier was changed from STA/DPE to ETE alone. The molar ratio of ETE to n-BuLi was 0.5:1. The Tg, microstructure of 25/75 SIR (styrene-isoprene rubber) formed and the time needed to consume more than 90 percent of the monomers charged are listed in TABLE 8.

Workup

  1. additioncontaining

Sources & evidence

ORD record
ord-1b598a28b7d443c89e4fff484b8bbda1
Source dataset
uspto-grants-1999_05
Patent number
US05906956