HuagongsheHuagongshe Chemistry Print Report · For research reference only
Styrene → 2-Methylbuta-1,3-diene;styrene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Butyllithium | HCID 178418339 | — |
| Product | 2-Methylbuta-1,3-diene;styrene | HCID 159989 | — |
Reaction Steps
The procedure described in Example 9 was utilized in this example except that a premix containing 25:75 mixture of styrene and 1,3-isoprene in hexanes was used in place of isoprene and the modifier was changed from STA/DPE to ETE alone. The molar ratio of ETE to n-BuLi was 0.5:1. The Tg, microstructure of 25/75 SIR (styrene-isoprene rubber) formed and the time needed to consume more than 90 percent of the monomers charged are listed in TABLE 8.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05906956 |
| Source dataset | uspto-grants-1999_05 |
| ORD ID | ord-1b598a28b7d443c89e4fff484b8bbda1 |
| Source note | uspto-grants-1999_05 |