HuagongsheHuagongshe Chemistry Print Report · For research reference only
Pentachlorophenol → HCID 86733441, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Pentachlorophenol | HCID 992 | — |
| Reactant | Pentaerythritol | HCID 8285 | — |
| Reactant | Triethyl phosphite | HCID 31215 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Catalyst | Iron | HCID 23925 | — |
| Product | HCID 86733441 | HCID 86733441 | — |
Reaction Steps
A 5-liter flask was charged with 1330 grams of pentachlorophenol, containing about 750 ppm of aluminum and iron compounds, 680 grams of pentaerythritol and 290 grams of triethylphosphite. The mixture was stirred and heated and volatiles were removed until the temperature was 145°C. Propylene oxide was then added until the acid number was less than 1. Since some solid materials was present 253 grams of pentachlorophenol was added and propylene oxide addition was continued until the acid number was less than 1. The mixture was stripped to remove volatiles and filtered through a coarse paper. The resulting oxypropylated polyol product weighted 3398 grams and had the following properties:
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US03957922 |
| Source dataset | uspto-grants-1976_05 |
| ORD ID | ord-7e33ffa7010843d2a0d27c618b3ed419 |