HuagongsheHuagongshe Chemistry Print Report · For research reference only
Acrylic Acid → Acrylic Acid
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Acrylic Acid | HCID 6581 | — |
| Reactant | Maleic Anhydride | HCID 7923 | — |
| Reactant | Potassium Persulfate | HCID 24412 | — |
| Reactant | Sodium | HCID 5360545 | — |
| Reactant | HCID 178418950 | HCID 178418950 | — |
| Reactant | HCID 178527019 | HCID 178527019 | — |
| Solvent | Water | HCID 962 | — |
| Product | Acrylic Acid | HCID 6581 | — |
| Product | Maleic Acid | HCID 444266 | — |
Reaction Steps
Copolymers of acrylic acid and maleic acid were prepared using sodium hypophosphite to promote telomerization. In a typical reaction, sodium hypophosphite monohydrate of a desired amount was added to deionized water and the solution heated to about 90°-100° C. Maleic anhydride was added to the solution and pH adjusted to about 4. Sodium or potassium persulfate (1-10% of total monomer feed) was used to initiate the polymerization. Acrylic acid at the appropriate ratio was added periodically over a 2-4 hour time period. Polymerization was continued until substantially 100% conversion was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05011682 |
| Source dataset | uspto-grants-1991_04 |
| ORD ID | ord-c98cd29c5e7b4ea687e948637397d90f |
| Source note | uspto-grants-1991_04 |