Acrylic Acid → Acrylic Acid
Reaction equation
[PH2]([O-])=O.[Na+].O.[PH2]([O-])=O.[Na+].C1(=O)[O:15][C:13](=[O:14])[CH:12]=[CH:11]1.[Na].S(OOS([O-])(=O)=O)([O-])(=O)=O.[K+].[K+].[C:30]([OH:34])(=[O:33])[CH:31]=[CH2:32]>O>[C:13]([OH:15])(=[O:14])[CH:12]=[CH2:11].[C:13]([OH:15])(=[O:14])/[CH:32]=[CH:31]\[C:30]([OH:34])=[O:33]Participants
9
Procedure
Copolymers of acrylic acid and maleic acid were prepared using sodium hypophosphite to promote telomerization. In a typical reaction, sodium hypophosphite monohydrate of a desired amount was added to deionized water and the solution heated to about 90°-100° C. Maleic anhydride was added to the solution and pH adjusted to about 4. Sodium or potassium persulfate (1-10% of total monomer feed) was used to initiate the polymerization. Acrylic acid at the appropriate ratio was added periodically over a 2-4 hour time period. Polymerization was continued until substantially 100% conversion was obtained.
Workup
- temperaturethe solution heated to about 90°-100° C
- customthe polymerization
- customPolymerization
- customwas obtained
Sources & evidence
- ORD record
- ord-c98cd29c5e7b4ea687e948637397d90f
- Source dataset
- uspto-grants-1991_04
- Patent number
- US05011682
Reaction notes
Loading…