HuagongsheHuagongshe Chemistry Print Report · For research reference only
Etidronic Acid → ZINC etidronate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Etidronic Acid | HCID 3305 | — |
| Reactant | Zinc Oxide | HCID 3007857 | — |
| Product | ZINC etidronate | HCID 86739934 | — |
Reaction Steps
First, 790 g of a solution of etidronic acid (158 g as etidronic acid) was heated to 70° C. and 461 g of a zinc oxide slurry (92.2 g as zinc oxide) held at 70° C. was added dropwise over about 30 minutes with constant stirring. The mol ratio of zinc oxide to etidronic acid was 1.5/1. This slurry was stirred at 60° to 70° C. for 4 hours, after which it was cooled to room temperature. The slurry was then filtered and the dehydrated cake was washed with distilled water 3 to 5 times. It was then filtered, dried and pulverized to give zinc etidronate.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04966630 |
| Source dataset | uspto-grants-1990_10 |
| ORD ID | ord-693616ad3a774054a7b8c320fe4be31f |
| Source note | uspto-grants-1990_10 |