Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1111430Generated: November 3, 2026

Azobisisobutyronitrile → Methyl Methacrylate

https://huagongshe.com/reaction/1111430

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAzobisisobutyronitrileHCID 6547—
ReactantEthylene glycol dimethacrylateHCID 7355—
ProductMethyl MethacrylateHCID 6658—
ProductEthyl MethacrylateHCID 7343—
Product2-Hydroxyethyl MethacrylateHCID 13360—

Reaction Steps

Into a test tube, were placed 50 g of polymerizable monomer containing silicon containing compound (A) obtained in Manufacturing Example 1, 25g of methyl methacrylate, 10 g of ethyleneglycol monomethacrylate, 5g of ethyleneglycol dimethacrylate, 10 g of ethyl methacrylate and 0.lg of azobisisobutyronitrile and after purging the air with nitrogen gas, the tube was sealed. The content was polymerized by UV irradiation at 40° C. for 18 hours and then by heating at 110° C. for 6 hours to obtain a colorless, solid stick, vinyl polymer containing silicon.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04980442
Source datasetuspto-grants-1990_12
ORD IDord-f5edbe4f453c42d381dee86da5007446