Methacrylic Acid → 2-Propenoic acid, 2-methyl-, polymer with 2-ethylhexyl 2-propenoate and methyl 2-methyl-2-propenoate
Reaction equation
[Cl-].[Na+].[C:3]([O:7][CH2:8][CH:9]([CH2:14][CH3:15])[CH2:10][CH2:11][CH2:12][CH3:13])(=[O:6])[CH:4]=[CH2:5].[C:16]([OH:21])(=[O:20])[C:17]([CH3:19])=[CH2:18].[C:22]([O:27][CH3:28])(=[O:26])[C:23]([CH3:25])=[CH2:24].C(S)CCCCCCCCCCC.C(OOC(=O)CCCCCCCCCCC)(=O)CCCCCCCCCCC>O>[C:3]([O:7][CH2:8][CH:9]([CH2:14][CH3:15])[CH2:10][CH2:11][CH2:12][CH3:13])(=[O:6])[CH:4]=[CH2:5].[C:16]([OH:21])(=[O:20])[C:17]([CH3:19])=[CH2:18].[C:22]([O:27][CH3:28])(=[O:26])[C:23]([CH3:25])=[CH2:24]Participants
8
Reactant 6
Product 1
Reagents, catalysts & solvents 1
Procedure
In 100 g of water placed in a 200 ml-volume flask were dissolved 0.1 g of polyvinyl alcohol (degree of polymerization of 1700 and degree of saponification of 88%) and then 4 g of sodium chloride. Into the solution were added 19.8 g of 2-ethylhexyl acrylate, 0.5 g of methacrylic acid, 1.25 g of methyl methacrylate, 0.005 g of dodecyl mercaptan, and 0.1 g of lauroyl peroxide. The mixture was allowed to polymerize at temperature of 60° C. for 6 hours. The resulting suspension particles were separated by filtration, washed with water and dried, to give 2-ethylhexyl acrylate/methacrylic acid/methyl methacrylate copolymer.
Workup
- customto polymerize at temperature of 60° C. for 6 hours
- customThe resulting suspension particles were separated by filtration
- washwashed with water
- customdried
Sources & evidence
- ORD record
- ord-65ba56f8de1849b0ae232259ae6d41e3
- Source dataset
- uspto-grants-1983_01
- Patent number
- US04367323
Reaction notes