HuagongsheHuagongshe Chemistry Print Report · For research reference only
Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | 1,3-Butadiene | HCID 7845 | — |
| Reactant | Cyclohexane | HCID 8078 | — |
| Reactant | Butyllithium | HCID 178418339 | — |
| Solvent | Methanol | HCID 887 | — |
| Product | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
Reaction Steps
In a polymerization vessel under nitrogen atmosphere were charged a cyclohexane solution containing 10 parts by weight of butadiene and 0.09 part by weight of n-butyllithium was added thereto. After polymerizing the mixture at 70° C. for 1 hour, a cylcohexane solution containing 90 parts by weight of styrene was added to the reaction mixture and polymerization reaction was continued at 70° C. for 2 hours. Thereafter, the polymerization reaction was stopped by adding methanol. The resulting polymer was separated from the polymer solution thus obtained by solidifying with methanol and then dried to obtain a styrene/butadiene block copolymer (weight average molecular weight: 100,000).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05110886 |
| Source dataset | uspto-grants-1992_05 |
| ORD ID | ord-2e2524bfc0d54bb7bae3c6da35d9520a |