Tetrasodium Pyrophosphate → HCID 86734064, compound
Reaction equation
[Cl-].[Ca+2:2].[Cl-].[O-:4][P:5]([O:8][P:9]([O-:12])([O-:11])=[O:10])(=[O:7])[O-:6].[Na+:13].[Na+].[Na+].[Na+]>>[OH2:4].[OH2:4].[OH2:4].[OH2:4].[O-:6][P:5]([O:8][P:9]([OH:12])([O-:11])=[O:10])(=[O:4])[O-:7].[Na+:13].[Ca+2:2]Participants
3
Procedure
A 25 weight percent aqueous solution of calcium chloride is added to a 15 weight percent aqueous solution of tetrasodium pyrophosphate in a suitable vessel until the pH reaches 7. The acicular crystals of calcium sodium pyrophosphate tetrahydrate are formed. The crystals are filtered, washed thoroughly, and dried at 60° C. The calcium sodium pyrophosphate tetrahydrate is then heated at a temperature within the range of 175° to 200° C for a period of 60 minutes until 3.2 moles of water of hydration is removed. The dehydrated solids were then ground. The structure of the material is now amorphous as determined by X-ray diffraction.
Sources & evidence
- ORD record
- ord-ad8ad2459f9846f5978bd2088315e930
- Source dataset
- uspto-grants-1976_10
- Patent number
- US03985675
Reaction notes