Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1421337Generated: October 25, 2026

Phosphoric Acid → Phosphate cerium nitrate

https://huagongshe.com/reaction/1421337

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPhosphoric AcidHCID 1004—
ReactantCerium nitrateHCID 24948—
ReactantBentoneHCID 56841936—
ReactantHCID 178526029HCID 178526029—
SolventWaterHCID 962—
ProductPhosphate cerium nitrateHCID 86755301—
ProductHCID 178526029HCID 178526029—

Reaction Steps

A clay/phosphate/cerium nitrate, vanadium oxalate slurry was prepared by adding 1340 grams of Theile RC-32® kaolin clay slurry to 1795 milliliters of water in a high speed mixer. To this mixture, 192 grams of phosphoric acid was added. Thereafter, 431 grams of cerium nitrate solution and 232 grams of vanadium oxalate solution were added to the slurry. The slurry was then spray dried and then resulting particles were calcined at 650° C. for 30 minutes in a muffle furnace. The calcined particles were then mixed with magnesium oxide in a 50/50 weight percent ratio and analyzed by TGA tests. These tests indicated that the resulting material produced an SOx absorption of 0.27% per minute.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06074984
Source datasetuspto-grants-2000_06
ORD IDord-cb4af3e3c8fb489bb52a91cf4a81a31b
Source noteuspto-grants-2000_06