Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Glycolide | HCID 65432 | — |
| Reactant | Lactide, L- | HCID 107983 | — |
| Solvent | Water | HCID 962 | — |
| Product | HCID 6453016 | HCID 6453016 | — |
Reaction Steps
An operation was conducted in the same manner as in Example 13 except that 22,050 g (glycolic acid: 70 ppm, glycolic acid dimer: 360 ppm, water: 20 ppm; overall proton concentration of impurities: 0.054 mol %) of glycolide and 450 g (lactic acid: 0 ppm, lactic acid dimer: 270 ppm, water: 8 ppm; overall proton concentration of impurities: 0.030 mol %) of L-lactide were used, and 2.06 g [in view of the amount (0.36 g) of water (moisture) contained in an atmosphere within the container] of water were added to control the overall proton concentration (set proton concentration) to 0.124 mol %. After completion of the polymerization, the yield of bulk matter of a poly(glycolic acid/L-lactic acid) copolymer formed was almost 100%. The bulk matter was ground by a grinder, and the physical properties of the ground product were measured. The results are shown in Table 5.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US07622546B2 |
|---|
| Source dataset | uspto-grants-2009_11 |
|---|
| ORD ID | ord-b871444c353547ca8baae072ae1d68f9 |
|---|
| Source note | uspto-grants-2009_11 |
|---|