Ethylene Oxide → Urethane acrylate
Reaction equation
[O:1]=[C:2]=[N:3]C1CC(C)(C)CC(C)(CN=C=O)C1.C([C:21]1C=C(C)C=C(C(C)(C)C)[C:22]=1[OH:32])(C)(C)C.C1OC1.C1OC1C.OCC[O:43][C:44](=[O:47])[CH:45]=[CH2:46]>>[C:44]([OH:47])(=[O:43])[CH:45]=[CH2:46].[NH2:3][C:2]([O:32][CH2:22][CH3:21])=[O:1]Participants
Procedure
To a reaction vessel equipped with a stirrer, 100 gm of ARONIX M113 manufactured by Toagousei Chemicals, 124.7 gm of isophorone diisocyanate, 1 gm of dibutyltindilaurate, and 0.3 gm of 2,6-di-t-butyl-4-methylphenol were added. To this, 842.7 gm of a copolymerization diol of ethylene oxide and 1,2-propylene oxide [ethylene oxide: 1,2 propylene oxide=2:8 (by weight)] of a number average molecular weight of 2,000 was added while maintaining the temperature in the 40° to 50° C. range, and the mixture was reacted for 2 hours. Then 32.6 gm of hydroxyethylacrylate was added, after which the mixture was continuously stirred for 5 hours at 50° to 60° C. to complete the reaction. A urethane acrylate [C-1] of a number average molecular weight of about 7,120 was obtained.
Workup
- customTo a reaction vessel equipped with a stirrer
- additionwere added
- additionwas added
- temperaturewhile maintaining the temperature in the 40° to 50° C. range
- customthe mixture was reacted for 2 hours
- customthe reaction
Sources & evidence
- ORD record
- ord-c828df3b600b4d9dbf7f412d84e7ce14
- Source dataset
- uspto-grants-1996_03
- Patent number
- US05496870