Ethylene Oxide → Urethane acrylate

https://huagongshe.com/reaction/1439983

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthylene OxideHCID 6354—
ReactantPropylene OxideHCID 6378—
Reactant2-Hydroxyethyl acrylateHCID 13165—
Reactant2,6-Di-tert-butyl-4-methylphenolHCID 31404—
ReactantIsophorone diisocyanateHCID 169132—
ProductUrethane acrylateHCID 21863578—

Reaction Steps

To a reaction vessel equipped with a stirrer, 100 gm of ARONIX M113 manufactured by Toagousei Chemicals, 124.7 gm of isophorone diisocyanate, 1 gm of dibutyltindilaurate, and 0.3 gm of 2,6-di-t-butyl-4-methylphenol were added. To this, 842.7 gm of a copolymerization diol of ethylene oxide and 1,2-propylene oxide [ethylene oxide: 1,2 propylene oxide=2:8 (by weight)] of a number average molecular weight of 2,000 was added while maintaining the temperature in the 40° to 50° C. range, and the mixture was reacted for 2 hours. Then 32.6 gm of hydroxyethylacrylate was added, after which the mixture was continuously stirred for 5 hours at 50° to 60° C. to complete the reaction. A urethane acrylate [C-1] of a number average molecular weight of about 7,120 was obtained.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05496870
Source datasetuspto-grants-1996_03
ORD IDord-c828df3b600b4d9dbf7f412d84e7ce14
Source noteuspto-grants-1996_03