Estradiol → Tetrahydrofuran toluene
Reaction equation
[CH3:1][C@@:2]12[C@@H](O)CC[C@H:15]1[C@H:14]1[C@@H:5]([C:6]3C=C[C:9]([OH:20])=[CH:10][C:11]=3CC1)[CH2:4][CH2:3]2.C1COCC1>C1(C)C=CC=CC=1>[C:2]1([CH3:1])[CH:15]=[CH:14][CH:5]=[CH:4][CH:3]=1.[CH2:10]1[CH2:9][O:20][CH2:6][CH2:11]1Participants
4
Reactant 2
Product 1
Reagents, catalysts & solvents 1
Procedure
Estradiol was combined with THF. Two parts by weight of polyethylenevinylacetate (PEVA) was combined with five parts by weight of poly-n-butyl methacrylate (PBMA) in toluene. The estradiol solution was combined with the PEVA/PBMA solution to form a coating solution containing 40 mg/ml total solids (30 wt. % estradiol, 20 wt. % PEVA, and 50 wt. % PBMA) and a solvent containing 80% toluene and 20% THF. The resulting solution was near the saturation point for estradiol in a solvent of 80% toluene and 20% THF at ambient temperature (approximately 21-22° C.).
Workup
- customto form a coating solution
- custom(approximately 21-22° C.)
Sources & evidence
- ORD record
- ord-5e9d2138d0c6484699f594b4bd77a931
- Source dataset
- uspto-grants-2016_08
- Patent number
- US09427501B2