反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
100 g of the thus obtained residue is heated with 50 g hydrolysis medium (90% lactic acid in aqueous solution) at 100° C. and atmospheric pressure for 4 hours with reflux and continuous thorough mixing. The resulting solution is mixed with sodium sulphide and, after 30 min thorough mixing, is filtered in order to remove solid material particles. The thus obtained, homogeneous solution has a lactic acid proportion of over 99% by weight and a racemisation degree of 2.5% and can be mixed with polycondensate in order to supply it directly to the depolymerisation unit. The total racemisation degree of the dilactide obtained after a plurality of cycles never rises, despite the recycling, above the maximum value which is achieved during direct depolymerisation up to a conversion of 95% (see example 1). The total yield is determined by the quantity which is removed during the hydrolysis by separation of the impurities and is preferably above 99%, however in any case more than 95%.
WORKUP
后处理
- temperatureatmospheric pressure for 4 hours with reflux
- filtrationis filtered in order
- customto remove solid material particles
- customThe thus obtained
- additiona racemisation degree of 2.5% and can be mixed with polycondensate in order to supply it directly to the depolymerisation unit