Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.C=CC=C>O1CCCC1>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1Participants
4
Reactant 2
Product 1
Reagents, catalysts & solvents 1
Procedure
In a 2 l reactor, styrene and butadiene was sequentially polymerizated using n-buthyllithium as initiator and tetrahydrofurane as polar modifier to obtain a styrene-butadiene living copolymer, that is made to react with Cl4Si as coupling agent for 5 min, obtaining so a SBS copolymer with a star shape, with four arms. The polymer had 29,7% of styrene, 42,5% of vinyl content in polybutadiene and a Mn=93400. The percentage of coupling was 96,5%.
Sources & evidence
- ORD record
- ord-39fa4f1a315e4cc68f3055bc47f7362f
- Source dataset
- uspto-grants-1999_11
- Patent number
- US05985995
Reaction notes