Molybdenum → Molybdenum oxide
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Molybdenum | HCID 23932 | — |
| Reactant | Azane;molybdenum;tetracosahydrate | HCID 25488 | — |
| Reactant | Phosphorus | HCID 5462309 | — |
| Reactant | Oxophosphanyl | HCID 6857426 | — |
| Solvent | Water | HCID 962 | — |
| Solvent | Phosphoric Acid | HCID 1004 | — |
| Solvent | Diammonium molybdate | HCID 61578 | — |
| Product | Azane;molybdenum;tetracosahydrate | HCID 25488 | — |
| Product | Molybdenum oxide | HCID 139765 | 51,545.102% |
Reaction Steps
A γ-alumina obtained as 1/16 inch extrudates from Criterion Catalyst Company L. P., Michigan City, Ind. was used. First, an ammonium heptamolybdate solution was prepared by dissolving (NH4)6Mo7O24 -4H2O in concentrated H3PO4 and water so that the ammonium molybdate concentration was 9.855 weight %, the H3PO4 concentration was 12.681 weight %, and water made up the rest. Then, 10 g of the alumina was impregnated at 25 ° C. with 5.32 g of the ammonium heptamolybdate solution to form a mixture. The mixture was then calcined in air at 538° C. for 6 hours to produce 10.18 g of a molybdenum oxide- and phosphorus oxide-impregnated alumina containing 2.807 weight % molybdenum and 2.096 weight % phosphorus (control catalyst).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06037302 |
| Source dataset | uspto-grants-2000_03 |
| ORD ID | ord-5a94a6f0c0c44d8690d7134a8519cc52 |
| Source note | uspto-grants-2000_03 |