Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1689567Generated: November 2, 2026

Urea → Strontium carbonate

https://huagongshe.com/reaction/1689567

Reaction equation

Participants

RoleNameHCIDCharge
ReactantUreaHCID 1176—
ReactantCarbonate IonHCID 19660—
ReactantStrontium nitrateHCID 24848—
ProductStrontium carbonateHCID 15407—
ProductCarbonate IonHCID 19660—

Reaction Steps

As shown in FIG. 1, a strontium nitrate (Sr(NO3)2) solution as a metal ion source was mixed in a container with a urea ((NH2)2CO) aqueous solution as a carbonate ion source to prepare a mixture solution containing 0.33M strontium nitrate and 0.33M urea. The container having the mixture solution was then placed into a reaction vessel and held at 90° C. for 90 minutes while agitating the mixture, whereby thermal decomposition of urea occurred to produce strontium carbonate crystals as the foregoing carbonate. The agitation was conducted at 500 rpm.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08153093B2
Source datasetuspto-grants-2012_04
ORD IDord-35ea0e59ffb847dc8caa13fdbb755e25
Source noteuspto-grants-2012_04