Urea → Strontium carbonate
Reaction equation
[N+]([O-])([O-])=O.[Sr+2:5].[N+]([O-])([O-])=O.NC(N)=O.[C:14](=[O:17])([O-:16])[O-:15]>>[C:14](=[O:15])([O-:17])[O-:16].[Sr+2:5].[C:14](=[O:15])([O-:17])[O-:16]Participants
5
Procedure
As shown in FIG. 1, a strontium nitrate (Sr(NO3)2) solution as a metal ion source was mixed in a container with a urea ((NH2)2CO) aqueous solution as a carbonate ion source to prepare a mixture solution containing 0.33M strontium nitrate and 0.33M urea. The container having the mixture solution was then placed into a reaction vessel and held at 90° C. for 90 minutes while agitating the mixture, whereby thermal decomposition of urea occurred to produce strontium carbonate crystals as the foregoing carbonate. The agitation was conducted at 500 rpm.
Workup
- customto prepare a mixture solution
- customwas then placed into a reaction vessel
Sources & evidence
- ORD record
- ord-35ea0e59ffb847dc8caa13fdbb755e25
- Source dataset
- uspto-grants-2012_04
- Patent number
- US08153093B2
Reaction notes
Loading…