HRID1729520
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
A sample vial was filled with 2 g of isopropoxy benzoyl chloride and SnCl4 was injected. The mixture was homogenized and then kept at the reaction temperature chosen. After the reaction 50 mg of the solidified red-brown reaction mixture was hydrolyzed in 1 ml of a mixture of CD3OD/D2O/NaOD (12:3:1, weight ratios) (2 hours, 60° C.) and the degree of polymerization (dp) was determined by NMR end-group analysis.
WORKUP
后处理
- customthe degree of polymerization (dp)