Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

HRID 1729839Notes

Reaction equation

HRID 1729839 reaction equation
[C:1](#[N:4])[CH:2]=[CH2:3].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1.C(OCC=C)(=O)C.C=CC>>[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1.[C:1](#[N:4])[CH:2]=[CH2:3]

Participants

5

Procedure

The reaction mixture is then stirred for 8 hours at 85°C. After cooling, the solvent and residual monomers are removed with steam and the reaction product is dried. 32.5 kg of a graft copolymer are obtained which has an ethylene/vinyl acetate copolymer content of 21.8 percent, by weight, an acrylonitrile content of 18 percent, by weight, a styrene content of 59 percent, by weight, an allyl acetate content of 0.9 percent, by weight, and a propylene content of 0.3 percent, by weight, (melt index at 190°C: 0.47). The following mechanical properties were determined:

Workup

  1. customby weight, (melt index at 190°C: 0.47)

Sources & evidence

ORD record
ord-292448e39b3d4c94888a7567f929e77a
Source dataset
uspto-grants-1976_11
Patent number
US03989770

Reaction notes

Loading…