Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

https://huagongshe.com/reaction/1729839

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantAcrylonitrileHCID 7855—
ReactantPropyleneHCID 8252—
ReactantAllyl acetateHCID 11584—
ProductProp-2-enenitrile--ethenylbenzene (1/1)HCID 62696—

Reaction Steps

The reaction mixture is then stirred for 8 hours at 85°C. After cooling, the solvent and residual monomers are removed with steam and the reaction product is dried. 32.5 kg of a graft copolymer are obtained which has an ethylene/vinyl acetate copolymer content of 21.8 percent, by weight, an acrylonitrile content of 18 percent, by weight, a styrene content of 59 percent, by weight, an allyl acetate content of 0.9 percent, by weight, and a propylene content of 0.3 percent, by weight, (melt index at 190°C: 0.47). The following mechanical properties were determined:

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS03989770
Source datasetuspto-grants-1976_11
ORD IDord-292448e39b3d4c94888a7567f929e77a
Source noteuspto-grants-1976_11