Water → HCID 67420429, compound
Reaction equation
[CH:1]#[C:2][C:3]1[CH:8]=[CH:7][C:6]([OH:9])=[CH:5][CH:4]=1.[CH:10](Cl)([CH3:12])[CH3:11].C(N(CC)CC)C.O>CC(C)=O>[OH:9][C:6]1[CH:7]=[CH:8][C:3]([CH:2]=[CH2:1])=[CH:4][CH:5]=1.[CH:10]([O:9][C:6]1[CH:7]=[CH:8][C:3]([CH:2]=[CH2:1])=[CH:4][CH:5]=1)([CH3:12])[CH3:11]Participants
6
Reactant 4
Product 1
Reagents, catalysts & solvents 1
Conditions
- Temperature
- 52.5 °C
Procedure
In 100 mL of acetone were dissolved 16.2 g of poly(p-hydroxystyrene) and isopropyl chloride. To this reaction mixture was added 1.8 g of triethylamine. This mixture was stirred at 50 to 55° C. for 5 hours. The resultant reaction mixture was transferred to 1,000 mL of water, and the upper layer was removed by decantation. The viscous resinous substance obtained was dissolved in 75 mL of acetone, and this solution was transferred to 500 mL of water. The rubbery resin precipitated was dried under vacuum. Thus, 15.4 g of poly(p-hydroxystyrene/p-isopropoxystyrene) was obtained as a white powder.
Workup
- customThe resultant reaction mixture
- customthe upper layer was removed by decantation
- customThe viscous resinous substance obtained
- customThe rubbery resin precipitated
- customwas dried under vacuum
Sources & evidence
- ORD record
- ord-2b589cc700b3411e8ab9872cb5abea2f
- Source dataset
- uspto-grants-2006_04
- Patent number
- US07022456B2
Reaction notes
Loading…