Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Sulfite | HCID 1099 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Product | HCID 19920498 | HCID 19920498 | — |
Reaction Steps
The hollow fiber contactor was used to treat condensate from a sulphite mill as described above. In this case, a 0.05 M NaOH solution was employed instead of nitrogen to remove the SO2 and other contaminants. A 2.0 L volume of this solution was re-circulated through the system. The feed solution and nitrogen flow rates were similar to those mentioned in Example III. Results are presented in Table V. About 98% removal for SO2 was achieved compared to 84% in Table II (after 4 hours using air). The BOD, COD and TOC reductions were 63%, 57%, and 54%, respectively. Higher NaOH concentrations would allow the concentration of SO2 produced in the form of NaHSO3/Na2SO3 to be significantly higher, if so desired. The NaHSO3/Na2SO3 solution could potentially be used within the mill or sold.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08349130B2 |
|---|
| Source dataset | uspto-grants-2013_01 |
|---|
| ORD ID | ord-68ed89538ff94350b6923c4ad90043c5 |
|---|
| Source note | uspto-grants-2013_01 |
|---|