Zinc sulfate monohydrate → Zinc Sulfate
Reaction equation
[S:1].O.[S:3]([O-:7])([O-:6])(=[O:5])=[O:4].[Zn+2:8].O.[S:10]([O-:14])([O-:13])(=[O:12])=[O:11].[Mg+2:15]>O>[S:1].[S:3]([O-:7])([O-:6])(=[O:5])=[O:4].[Zn+2:8].[S:10]([O-:14])([O-:13])(=[O:12])=[O:11].[Mg+2:15]Participants
7
Procedure
The mill base is prepared by milling a mixture of Sulphur (30%), Zinc sulphate monohydrate (50%) and Magnesium sulphate monohydrate (10%) Naphthalene sulfonate condensate (Tammol DN) (4%) Lignin sulfonate (Reax 100) (5%), and Napthalene sulfonate (1%) and the mixture is spray granulated as in Example 1 to get water dispersible granules of Sulphur 30%+Zinc Sulphate 50%+Magnesium sulphate 10%.
Workup
- customThe mill base is prepared by milling
Sources & evidence
- ORD record
- ord-87cefd0b277b4e879541b8d169119696
- Source dataset
- uspto-grants-2015_02
- Patent number
- US08951327B2
Reaction notes
Loading…