Hydrochloric Acid → Zirconium(IV) sulfate
Reaction equation
O(Cl)Cl.[Zr:4].[S:5]([O-:9])([O-:8])(=[O:7])=[O:6].[Na+].[Na+].Cl>>[S:5]([O-:9])([O-:8])(=[O:7])=[O:6].[Zr+4:4].[S:5]([O-:9])([O-:8])(=[O:7])=[O:6]Participants
4
Conditions
- Temperature
- 75 °C
Procedure
625 g of a 16% (ZrO2 conversion) zirconium oxychloride solution at room temperature was added to 237 g of a 25% sodium sulfate solution. After addition of hydrochloric acid to achieve a free acid concentration of 1.5 N, this was heated to 75° C. and maintained for 1 hour to age while producing basic zirconium sulfate.
Workup
- temperaturemaintained for 1 hour to age