Triethylene Glycol → HCID 86607620, compound
Reaction equation
[CH2:1]([OH:10])[CH2:2][O:3][CH2:4][CH2:5][O:6][CH2:7][CH2:8][OH:9].[CH3:11][N:12]1[CH2:16][CH2:15][CH2:14][C:13]1=[O:17]>>[CH3:11][N:12]1[CH2:16][CH2:15][CH2:14][C:13]1=[O:17].[CH2:1]([OH:10])[CH2:2][O:3][CH2:4][CH2:5][O:6][CH2:7][CH2:8][OH:9].[OH2:3]Participants
Procedure
Polyethersulfone (SUMIKAEXCEL®4800P, manufactured by Sumika Chem Tex Co., Ltd.) (20 mass %), triethyleneglycol (manufactured by MISTUI CHEMICALS, INC.) (40 mass %), and N-methyl 2-pyrrolidone (manufactured by Mitsubishi Chemical Corporation) (40 mass %) were mixed and stirred to prepare a homogeneous and transparent membrane-forming solution. A hollow fiber membrane was obtained in the same manner as in Example 2, except that this membrane-forming solution and N-methyl 2-pyrrolidone/triethyleneglycol/water (=5/5/90) as a void-forming material were used. The inner diameter of the hollow fiber membrane was 195 μm; the thickness thereof was 51.5 μm; the moisture content thereof was 0.4 mass %; and the mass ratio of the hydrophilic polymer was 0 mass %.
Workup
- customto prepare a homogeneous and transparent membrane-forming solution
Sources & evidence
- ORD record
- ord-457c49a2e85b467292e110dd5d921cbc
- Source dataset
- uspto-grants-2009_12
- Patent number
- US07638052B2
Reaction notes
Loading…