HRID1912241

反应详情

EQUATION

反应方程式

HRID 1912241 的结构方程式

PROCEDURE

实验过程

A mixture of 90 parts by mass of PET obtained above and 10 parts by mass of silicon dioxide (“Silysia 445,” average particle size 2.5 μm, manufactured by Fuji Silysia Chemical Ltd.) was kneaded at 260° C. using a vented counter-rotation twin-axis extruder (L/D=35) with 30 mmφ, to prepare a PPT master (MS-4) containing 10% by mass of silicon dioxide.

WORKUP

后处理

  1. customwas kneaded at 260° C.