HuagongsheHuagongshe Chemistry Print Report · For research reference only
Phosphorus oxychloride → HCID 23209276, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Phosphorus oxychloride | HCID 24813 | — |
| Reactant | HCID 178469536 | HCID 178469536 | — |
| Product | HCID 23209276 | HCID 23209276 | — |
Reaction Steps
A mixture of ethyl 6-ethyl-4-hydroxy-1,5-naphthyridine-3-carboxylate (3.0 g) and phosphorus oxychloride (25 ml) was stirred and heated at 40°-50° C. for 1 hour. The mixture was then cooled and then worked up as described in Example B1 to give ethyl 4-chloro-6-ethyl-1,5-naphthyridine-3-carboxylate, m.p. 94°-96° C.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05780482 |
| Source dataset | uspto-grants-1998_07 |
| ORD ID | ord-87ceb326d7d448498b7332ab8dea9228 |
| Source note | uspto-grants-1998_07 |